Ave._out Min._out Max._out Ave.mo Min.mo Max.mo 1 0.06324 0.00001 0.16450 0.32371 0.04649 0.44124 2 0.61835 0.00016 0.95659 0.44471 0.06421 0.61592 3 0.74924 0.00565 0.99975 0.58402 0.12196 0.77764 4 0.79108 0.16439 1.00000 0.72032 0.32686 0.86994 5 0.96792 0.87168 1.00000 0.85695 0.69865 0.91989 6 0.99894 0.99574 1.00000 0.92306 0.88376 0.94307 7 0.99996 0.99983 1.00000 0.94433 0.93397 0.95396 8 1.00000 0.99999 1.00000 0.95411 0.95069 0.96061 9 1.00000 1.00000 1.00000 0.95887 0.95426 0.96450 10 1.00000 1.00000 1.00000 0.96149 0.95644 0.96692 11 1.00000 1.00000 1.00000 0.96293 0.95771 0.96836 12 1.00000 1.00000 1.00000 0.96391 0.95823 0.96942 13 1.00000 1.00000 1.00000 0.96452 0.95836 0.97045 14 1.00000 1.00000 1.00000 0.96490 0.95837 0.97121 15 1.00000 1.00000 1.00000 0.96513 0.95836 0.97173 16 1.00000 1.00000 1.00000 0.96530 0.95842 0.97216